ZRC Galvilite® Galvanizing Repair
- Designed specifically for field and shop repair of hot dip galvanizing
- Silver finish closely blends in with the color of new hot dip galvanizing
- Meets and exceeds galvanizing repair specifications ASTM Des. A 780, SSPC-Paint 20 and DOD-P-21035A
- Industry-leading 95% zinc in the dried film
- Single-component
- Apply by brush, roller or spray
- Meets VOC standards in all 50 states
- Available in clog-free aerosol form
Specifications
TYPE: Single pack, premixed, ready-to-apply, liquid organic zinc compound with a shiny finish to closely approximate the color of hot-dip galvanizing
GENERAL PROPERTIES: Galvilite® is a high-quality cold galvanizing compound based on a trade secret organic binder which affords true galvanic anti-corrosion protection to metals. The dried film of GALVILITE is 95% metallic zinc. Because of the uniqueness of the formulation, GALVILITE is the only coating of its type to be recognized under the Component Program of Underwriter's Laboratories, Inc.
RECOMMENDED USES: Galvilite is widely used without topcoat in place of hot-dip galvanizing. Specially formulated for repair of damaged hot-dip galvanizing Galvalume® and zinc metallizing, regalvanizing worn hot-dip galvanizing, repair of weldments, and repair of damaged inorganic zinc coatings. Excellent for long-term protection of structural steel, water and waste facilities, power plants, transmission towers and antennae, steel decking and bridges, and numerous OEM uses.
SUBSTRATES: Apply to properly prepared carbon steel, cast iron, hot-dip galvanized, and aluminum surfaces
GENERAL PROPERTIES: Galvilite® is a high-quality cold galvanizing compound based on a trade secret organic binder which affords true galvanic anti-corrosion protection to metals. The dried film of GALVILITE is 95% metallic zinc. Because of the uniqueness of the formulation, GALVILITE is the only coating of its type to be recognized under the Component Program of Underwriter's Laboratories, Inc.
RECOMMENDED USES: Galvilite is widely used without topcoat in place of hot-dip galvanizing. Specially formulated for repair of damaged hot-dip galvanizing Galvalume® and zinc metallizing, regalvanizing worn hot-dip galvanizing, repair of weldments, and repair of damaged inorganic zinc coatings. Excellent for long-term protection of structural steel, water and waste facilities, power plants, transmission towers and antennae, steel decking and bridges, and numerous OEM uses.
SUBSTRATES: Apply to properly prepared carbon steel, cast iron, hot-dip galvanized, and aluminum surfaces
NOT RECOMMENDED FOR: Contact with potable water, strong acids or strong alkalis
TEMPERATURE RESISTANCE (non-immersion):
Continuous: 350°F max/177°C max
Non-Continuous: 750°F max/399°C max
SALT FOG EXPOSURE: 2,852 Hours (ASTM B117)
PROHESION/QUV EXPOSURE: 2,000 Hours (ASTM D5894)
VOC: 3.3 Lbs/gal (385 gms/Ltr) (ASTM D3960)
PROJECT SPECIFICATIONS:
TEMPERATURE RESISTANCE (non-immersion):
Continuous: 350°F max/177°C max
Non-Continuous: 750°F max/399°C max
SALT FOG EXPOSURE: 2,852 Hours (ASTM B117)
PROHESION/QUV EXPOSURE: 2,000 Hours (ASTM D5894)
VOC: 3.3 Lbs/gal (385 gms/Ltr) (ASTM D3960)
PROJECT SPECIFICATIONS: